ASTM F2516 Tensile Testing of Nitinol Wire
ASTM F2516 measures the tensile properties of superelastic nickel-titanium or Nitinol. The material properties of nitinol are different from those of most other materials – nitinol will change its structure depending on its temperature or the amount of stress applied to it. This means that it will exhibit very different stress strain profiles during loading and unloading, which is why this standard captures both an upper and lower plateau strength, rather than a singular yield strength. The ASTM F2516 test method is designed to pull the material in tension to 6% strain, then unload the material to a value of less than 7MPa before being pulling it to failure.
- Metals
- Biomedical
- Tension
- Compression
- ASTM F2516
Nitinol's unique properties mean that it is used extensively in the biomedical industry to create stents, dental wires, catheter guidewires, internal fracture fixation devices, and biopsy forceps. One of its properties - shape memory - enables it to "remember" its shape when formed at a certain temperature. When the temperature is lowered beyond this point Nitinol can be molded to any other shape, but will automatically revert to its original shape once it reaches the temperature at which it was initially formed. This property makes it extremely useful for the creation of stents, which are used to hold open blood vessels and prevent severe clots. The stent can be transported through the body to the target location in a compacted form, reforming to its original cylindrical form once it warms up to body temperature at the target location. Nitinol is also commonly used for braces – the Nitinol is molded into the desired final shape, and the temperature within the mouth stresses the material to reform, slowly adjusting the teeth into their ideal positions. Unlike more traditional braces, nitinol braces wire is especially beneficial because it does not require frequent retightening.
Test SetupASTM F2516 is typically performed on a dual column materials testing system such as Instron's 6800 Series. A 5 kN load cell is most likely appropriate for most materials. Bluehill Universal software with TestProfiler is also required, and the test method for ASTM F2516 comes pre-loaded in Bluehill Universal's Biomedical Applications Module.
ASTM F2516 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2714-005 Pneumatic Cord and Yarn Grips |

The gripping solution is dictated by specimen diameter, with most small diameters being tested with pneumatic cord and yarn grips and larger diameters utilizing pneumatic side action grips with serrated faces.
The diameter of the wire being tested determines the extensometry class required. For any wire 0.2 mm or smaller in diameter, crosshead movement can be used for strain measurement. Diameters greater than 0.2mm require a class C extensometer, with Instron's AUTOX automatic contacting extensometer, and AVE2 non-contacting extensometers being popular choices, as the weight of clip-on devices can affect results when testing such small specimens.
Specimen diameter and gauge length also determine test speed, so utilizing expression builder in Bluehill Universal can provide an easy way to update the test speed automatically. The lab temperature for this test is also very important - the material needs to be tested at a temperature at least 5 degrees higher than its austenitic finish transformation temperature. If not, the material will be partially transformed to a different material state, affecting the results.
Related Content6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
3400 Series - Affordable Testing Solutions
Instron 3400 Series Universal Testing Systems for Tensile, Compression, Bend, and other material property tests.
Bluehill Universal Brochure
Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.
TestProfiler for Bluehill Universal
2712-04X Series Pneumatic Side-Action Grips
Pneumatic side-action grips offer a versatile gripping solution for a wide range of materials. Rated capacities between 1 and 10 kN.
2714-005 Pneumatic Cord and Yarn Grips
Pneumatic cord and yarn grips provide a convenient method for clamping fiber, cord, yarns and fine wires to reduce the problem associated with testing these materials. Rated capacity 1 kN.
AVE 2 Non-Contacting Video Extensometer
The second generation Advanced Video Extensometer (AVE 2) utilizes patented measurement technology in the fastest, most accurate non-contacting strain measurement device commercially available.
Automatic Contacting Extensometer - Model AutoX 750
The AutoX 750 is a high-resolution, long-travel automatic contacting extensometer. It can be mounted onto any electromechanical 3300, 3400, 5500, 5900, or 6800 Series tabletop or floor model system as well as LX, DX, HDX, and KPX static hydraulic testing systems. It is well suited for applications involving plastics, metals, biomedical, composites, elastomers, and more. The AutoX has a maximum travel of 750 mm and accuracy of ± 1 µm.