ASTM D1037, the Standard Test Method for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials, outlines multiple testing procedures to characterize the mechanical properties of fiberboard. The internal bond test procedure is outlined in section 11 of the ASTM D1037 standard, though other sections also evaluate fastener holding, flexure properties, and compression properties in ambient or simulated environmental conditions.
Wood fiberboard is an engineered material made by using an adhesive to glue wood chips or wood particles together under high pressure, and the internal bond test of ASTM D1037 ensures that the cohesion strength of the engineered panel is sufficient for a given application. The internal bond test measures the tensile strength of the material when applying a force perpendicular to the face. This testing is especially important considering that these materials are used in construction applications and many of them are formed through the adhesion of multiple layers of material.
Most ASTM D1037 force requirements are suitable for a dual column universal testing system such as those found in Instron's 6800 and 3400 Series. Required fixtures include Instron's 2820-061 internal bond test fixture and 2820-062 steel specimen blocks, which were designed in compliance with the requirements of this standard.
ASTM D1037 | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2820-061 Internal Bond Fixture for Wood and Fiberboard |

The principle of ASTM D1037 internal bond testing involves bonding specimen blocks to the top and bottom surfaces of the test specimen with a suitable adhesive. The loading block bond must be stronger than the expected failure force of the specimen. The upper loading fixture should be self-aligning, and the specimen blocks should be 2-inch square by 1-inch in thickness and made from steel or aluminum alloy. Instron’s 2820-061 and 2820-062 fixtures have been designed in compliance with these requirements.
Related Content6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
3400 Series - Affordable Testing Solutions
Instron 3400 Series Universal Testing Systems for Tensile, Compression, Bend, and other material property tests.
Bluehill Universal Brochure
Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.
2820-061 Internal Bond Fixture for Wood
The 2820-061 internal bond fixture is designed for testing the strength properties of wood or adhesive bonds in wood by tensile loading.