ASTM D5035 Breaking Strength and Elongation of Textile Fabrics (Strip Method)
TIPS AND TRICKS
- This standard recommends a Constant Rate of Extension (CRE) frame for testing, however, it also notes that Constant Rate of Load or Constant Rate of Traverse are acceptable as well. When different testing machines are used for testing the same materials, a constant time-to-break of 20 +/- 3 seconds is recommended for the most comparable results. It should be noted that results still can vary significantly based on the frame used.
- ASTM D5035 requires that two sets of specimens are prepared, one in the warp direction and one in the weft direction.
- Instron’s Bluehill Universal testing software has advanced pre-built methods available with pre-configured calculations helping to ensure compliance to ASTM D5035.
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
Bluehill Universal Brochure
Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.
2712-04X Series Pneumatic Side-Action Grips
Pneumatic side-action grips offer a versatile gripping solution for a wide range of materials. Rated capacities between 1 and 10 kN.