The electric vehicle battery industry is constantly improving the energy density and safety of their products. A significant focus is on the aluminum and copper foils used in each cell as current collectors. Thinner foil helps to reduce battery weight (contributing to energy density), and longer/wider foil increases production efficiency (contributing to cost reduction). However, as innovation drives foil materials to become thinner, it becomes even more critical to accurately capture their material properties and ensure that adequate quality control measures are in place.

Many companies in the industry are currently working on producing copper foil between 4 and 12 microns thick. However, as copper foil becomes thinner, longer, and wider, improved technology is required to address wrinkling and tearing concerns during production. Given that batteries need to be able to withstand the mechanical loading under normal use, as well as expansion and contraction when charging and discharging over time, the current collector foil must also be able to withstand these factors without yielding. Ensuring that these newer foils are able to withstand the loads required of it during both use and production, increased mechanical testing is needed.

Relevant standards for this application include ASTM E345, EN 546-2, and DIN 50154, which can be used as guidance for testing EV battery foils.

A standard tensile test is the most appropriate way to determine the mechanical properties of aluminum and copper foil specimens. Typically, elongation at break and maximum load are the key material properties that are calculated in mechanical testing, as these properties help ensure the quality of the foil; whether or not it will be able to withstand the mechanical loading and expansion/contraction in use.

While some standards may call out gripping options, such as wedge action grips, Instron has found that pneumatic side action grips are the optimal solution for foil under 20 microns thick. Pneumatic side action grips offer the ability to fine tune the clamping pressure and they will always provide constant pressure throughout each test. The use of pneumatic grips also improves throughput for these high-volume materials, as quality control labs can test hundreds of specimens per day. An additional factor that must be considered is the type of clamping surface, such as the jaw faces used. The optimal jaw faces to pair with pneumatic side action grips are rubber-coated faces. The soft and pliable rubber is able to adequately hold foil material throughout the duration of a test, while minimizing the stress concentration added by clamping the specimens.

foil testing in universal testing machine

 

Two of the biggest challenges that come from testing foil material are the preparation and alignment of the specimen. Specimen preparation is extremely critical for such fragile specimens. The better the quality of the cut, the better the quality of the edges will be for each specimen. Poorly cut edges increase the chances of the material breaking prematurely. Premature failure reduces the quality of the test results, and can lead to the need for re-testing.

Specimen alignment is also critical for repeatability and protection of the specimen, as thin foils can be noticeably affected by minor misalignment within the grips. Additionally, having to adjust foils within the grips multiple times can sometimes lead to premature breaks due to the damage caused by clamping and unclamping. We highly recommend using Instron’s Precision Specimen Loader to reduce variability in test results while improving ergonomics and safety.

Automation systems from Instron introduce a new level of productivity for foil testing. As battery production volumes continue to increase, throughput and efficiency are critical to keep up with demand. Utilizing an automation system with the recommended equipment for each application can free up operators and maximize throughput, while maintaining optimal results.

Related Content
EV White Paper

电动汽车动力电池材料测试白皮书

静态力学材料测试是评估电动汽车安全性和可靠性的关键。电动汽车销量飙升,加上电池技术不断变化,导致需要经历整套测试流程的零部件和材料种类不断扩大。本白皮书探讨了与电动汽车动力电池应用相关的重要的静态力学材料测试方法及技术。

EV E-Guide

如何为你的电动汽车的动力电池选择最适合的材料测试设备

力学材料测试是评估电动汽车(EV)电池系统性能和安全的关键。准确、高效、安全的材料测试设备对于那些试图在这个竞争激烈的新行业中提高生产力并缩短上市时间的公司来说至关重要。该手册将引导你如何通过三个关键步骤,为电动汽车动力电池的应用选择最合适的测试设备。

Precision Specimen Loader

The Precision Specimen Loader for Thin Films provides a safer, more ergonomic, accurate, and more convenient way to load thin film and foil specimens into Instron 2712-052 grips.

EV White Paper

电动汽车动力电池材料测试白皮书

静态力学材料测试是评估电动汽车安全性和可靠性的关键。电动汽车销量飙升,加上电池技术不断变化,导致需要经历整套测试流程的零部件和材料种类不断扩大。本白皮书探讨了与电动汽车动力电池应用相关的重要的静态力学材料测试方法及技术。

6800 系列 - 万能材料试验系统

Instron 的6800 系列万能材料试验系统提供出色的精度及可靠性。 6800 系列基于正在申请专利的操作员保护架构,具有全新的智能气动控制装置和碰撞保护功能,使材料测试比以往任何时候都更简单、更智能、更安全。

3400 系列 - 万能材料试验系统

Instron 的 3400 系列万能材料试验系统,可用于材料的拉伸、压缩、弯曲以及其它性能测试。

Bluehill Universal 手册

Bluehill Universal 软件专为直观的触摸交互式用户体验而构建。通过预加载试验方法、数秒内的QuickTest、增强数据导出,以及 Instron Connect(一项可与服务工程师直接联系的新功能)等功能去探索更简单、更智能的测试方式。Bluehill 2、 Bluehill 3 等旧版本软件的用户可以轻松升级到最新版本的 Bluehill。

2712-04X 系列气动平推夹具

气动平推夹具适用于各种材料和试样的静态拉伸试验。其载荷范围在 1 至 10 kN之间。

Contact Us

請填妥以下表格,我們將很樂意與您聯絡。通常我們回覆線上請求的時間是 1-2 個工作天。如要更快取得回覆,請致電聯絡我們,來電話撥打以下號碼。

銷售: +886 35 722 155
服務: +886 35 722 155

服務請求

針對服務相關問題,請按以下按鈕並填妥聯絡表格。

请输入您的电子邮箱地址 邮箱中必须包含@符号 邮箱地址只能包含字母,数字和以下特殊符号: . ! # $ % & ' * + - / = ? ^ _ ` { | } ~ 邮箱地址域名只能包含字母,数字,圆点(.)和连接符(-)
请输入您的留言信息 邮箱地址只能包含字母,数字和以下特殊符号: . ! # $ % & ' * + - / = ? ^ _ ` { | } ~
下一步 检查您是否是旧访客...

欢迎回来!

您的联系信息

请输入您的名字
请输入您的姓氏
请选择您的国籍
请输入您的公司名称
请输入您的地址
请输入您的地址2
请输入您的地址3
请选择您所在的国家
请输入您的城市
请选择您的州/省
请输入您的邮政编码
请输入您的电话号码

请确定您同意英斯特朗隐私和 Cookie政策的条款与条件并提交

我同意英斯特朗隐私和 Cookie政策的条款与条件
请选择订阅服务 您有一个或多个空白处,请完成表格并继续 您有一处或多处格式错误,请解决错误并继续 请确定您同意英斯特朗隐私和 Cookie政策的条款与条件并提交