BS EN 1719 Tack Measurement for Pressure Sensitive Adhesives

envelopes and tensile grips

BS EN 1719 determines the “loop tack” measurement for coated pressure-sensitive adhesives. This standard is primarily used by manufacturers of paper and board, packaging, and disposable sanitary products to measure the strength of things such as envelope adhesives and diaper tab adhesives. To create specimens for this test, adhesive strips are formed into a loop and gripped together. The adhesive loop is brought down into contact with a flat rigid plate at a rate of 5 mm/s. When the loop contacts the plate over approximately 25 mm by 25 mm, the adhesive loop is pulled upwards at a rate of 5 mm/s and the maximum force to fully separate the loop from the plate is recorded.

Materials Testing System

Instron’s 6800 Series frames enable data capture of up to 2.5 kHz to ensure that all fast-changing test events are captured. Too low of a bandwidth may “dull” the results and lead to a missed peak, resulting in artificially lower loop tack values. System capacity will depend on the strength of the elastomer; however most tests to this standard will be very low force, making this application perfect for a single column frame (34SC or 68SC).  




BS EN 1719 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2712-041 Pneumatic Side Action Grips

 

materials testing system
Grips

Pneumatic side action grips prevent specimen slippage by maintaining a constant clamping pressure throughout testing. These are available in capacities from 50 N up to 10 kN, but BS EN 1719 only requires the very lowest end of this force spectrum. Both pneumatic and advanced side action grips feature quick-change jaw faces that can be easily changed to accommodate different materials.

50 N Model | 2712-051
2712-052
250 N Model | 2712-052
Testing Tips and Tricks
  • Bluehill Universal is provided with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards, including BS EN 1719, which is part of the Adhesives module. Please note that this method requires the use of TestProfiler.
  • To read this standard in full, purchase BS EN 1719.
Related Content

6800 系列 - 万能材料试验系统

Instron 的6800 系列万能材料试验系统提供出色的精度及可靠性。 6800 系列基于正在申请专利的操作员保护架构,具有全新的智能气动控制装置和碰撞保护功能,使材料测试比以往任何时候都更简单、更智能、更安全。

3400 系列 - 万能材料试验系统

Instron 的 3400 系列万能材料试验系统,可用于材料的拉伸、压缩、弯曲以及其它性能测试。

Bluehill Universal 手册

Bluehill Universal 软件专为直观的触摸交互式用户体验而构建。通过预加载试验方法、数秒内的QuickTest、增强数据导出,以及 Instron Connect(一项可与服务工程师直接联系的新功能)等功能去探索更简单、更智能的测试方式。Bluehill 2、 Bluehill 3 等旧版本软件的用户可以轻松升级到最新版本的 Bluehill。

2712-04X 系列气动平推夹具

气动平推夹具适用于各种材料和试样的静态拉伸试验。其载荷范围在 1 至 10 kN之间。

2710 系列手动平推夹具

手动平推夹具提供了一种简单有效的夹持试样的方法,可以广泛应用于各类试验。