Instron

제품소개 » 액세서리 » Application Specific Fixtures » 식품 고정 장치 » Puncture Probe Set, Magness-Taylor

Puncture Probe Set, Magness-Taylor

Catalog no. 2830-005

Magness-Taylor Puncture Probe
Magness-Taylor Puncture Probe

2830-015 | Puncture Probe Set, Magness-Taylor

Includes probes of 7.9 mm (0.31 in) and 11.1 mm (0.44 in) diameter.

Upper fitting: Requires Chuck 2830-036.

Lower fitting: Requires optional support plates with Drip tray S5400A and Support Frame S4427A.

문헌

Food Texture Fixtures Probes and Chucks

Flat-end puncture probes produce a shear stress in the specimen. The force required to cause shearing as the probe penetrates the specimen relates to texture properties such as firmness and hardness.

  • 제품소개
  • 11/06/2018
  • 686.36 KB

관련 항목
사양표