2716-111 | Pneumatic Wedge Action Grips

Capacity: 100 kN (20,000 lb, 10,000 kg)

Upper and lower fittings: Type Dm (1.25 in connection with 1/2 in clevis pin)

Maximum specimen thickness: 40 mm (flat)

Maximum specimen width: 75 mm (flat)

Maximum specimen diameter: 50 mm (round)

Clamping length: 70 mm

Temperature range: ambient only

Requires faces

Includes an air distribution kit with both, 1/4 NPTM (7/16-20), and 1/4 inch hose barb end connections

An Automatic Air Control Kit or Footswitch is recommended

문헌

2716 Series Pneumatic Wedge Action Grips Data Sheet

The Pneumatic Wedge Action Grips, available in 100 or 200 kN, provide a convenient method of clamping both large round and flat specimen shapes, up to a 50 mm (2 in) diameter, or flat specimens up to 40 mm (1.57 in) thick respectively. V-face grips are used for round specimens by design and have a reduced area at the center that compromises their ability to absorb high-energy breaks without fracture. This grip uses a split V-face configuration that allows the break energy to be dissipated without damaging the faces.