ASTM D3330: Test Method for Peel Adhesion of Pressure-Sensitive Tape

ASTM D3330 is a major peel testing standard that outlines the requirements for determining the peel adhesion properties of pressure-sensitive tapes such as surgical, electrical, packing, and duct tape. The standard includes 6 different methods (A-F) for measuring peel adhesion with both 90° and 180° peel tests. This guide is designed to introduce you to the basic elements of ASTM D3330 testing, including an overview of the equipment, software, and specimens needed.

Learn more about ASTM D3330.