ISO 36 Adhesion to Textile Fabrics

ISO 36 determines the strength required to separate two plies of fabric bonded together with rubber, or a rubber and a fabric ply bonded together.  This test is referred to as a “T-peel” test, because as the two adherends are pulled apart, they form the shape of a “T”.  Specimens for ISO 36 are 25 mm wide and are pulled apart at 50 mm/min for a minimum separation of 100 mm.  Common results are the average, minimum and maximum peel force and peel strength values.

The challenges of testing to this standard are:

  • Data rate used to capture peaks and troughs
  • Gripping materials of varying thickness
  • Eliminating slippage throughout the test

Instron Solution:

  • Data rate used to capture peaks and troughs – Instron’s 6800 series frames enable data capture of up to 2.5 kHz to ensure that all fast changing test events are captured.  Too low of a bandwidth may “dull” the system and lead to missed peaks and troughs, resulting in lower average strength values.
  • Gripping materials of varying thickness – When testing an adhesive on a thick substrate, standard grips can result in a misaligned specimen.  The advanced screw action grips can be adjusted to offset and ensure that the specimen remains centered in the load string.
  • Eliminating slippage throughout the test – The advanced screw action grips employ a patented “quick-change” jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials.  Pneumatic grips can also be used and are able to maintain consistent gripping pressure throughout the test.

It is important to review ISO 36:2011 in order to fully understand the test setup, procedure, and results requirements.

 

Literature

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • 产品
  • 02/10/2020
  • 1.93 MB

2710 Series Screw Side Action Grips

Screw side-action grips provide a very simple and efficient method for holding test specimens in a wide range of applications. The dual – acting design of 2710-100 series grips means that jaw faces can be adjusted to accommodate different specimen thicknesses. This ensures that the line of tensile force remains concentric with the grip body. They can be equipped with a selection of interchangeable grip jaw faces in various sizes and choice of surfaces including smooth ground, rubber-coated and serrated. Line contact and special coated faces are also available.The unique ‘snap-on’ jaw face attachment makes changing faces extremely quick and simple.

  • 产品
  • 06/28/2017
  • 1.29 MB

2712-04X Series Pneumatic Side-Action Grips

Pneumatic side-action grips offer a versatile gripping solution for a wide range of materials. Rated capacities between 1 and 10 kN.

  • 产品
  • 03/22/2022
  • 1.13 MB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability

  • 产品
  • 02/26/2017
  • 3.77 MB