ISO 36 Adhesion to Textile Fabrics
ISO 36 determines the strength required to separate two plies of fabric bonded together with rubber, or a rubber and a fabric ply bonded together. This test is referred to as a “T-peel” test, because as the two adherends are pulled apart, they form the shape of a “T”. Specimens for ISO 36 are 25 mm wide and are pulled apart at 50 mm/min for a minimum separation of 100 mm. Common results are the average, minimum and maximum peel force and peel strength values.
The challenges of testing to this standard are:
- Data rate used to capture peaks and troughs
- Gripping materials of varying thickness
- Eliminating slippage throughout the test
Instron Solution:
- Data rate used to capture peaks and troughs – Instron’s 6800 series frames enable data capture of up to 2.5 kHz to ensure that all fast changing test events are captured. Too low of a bandwidth may “dull” the system and lead to missed peaks and troughs, resulting in lower average strength values.
- Gripping materials of varying thickness – When testing an adhesive on a thick substrate, standard grips can result in a misaligned specimen. The advanced screw action grips can be adjusted to offset and ensure that the specimen remains centered in the load string.
- Eliminating slippage throughout the test – The advanced screw action grips employ a patented “quick-change” jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials. Pneumatic grips can also be used and are able to maintain consistent gripping pressure throughout the test.
It is important to review ISO 36:2011 in order to fully understand the test setup, procedure, and results requirements.
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Produkte
- 02/10/2020
- 4.15 MB
2710 Series Screw Side Action Grips
Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.
- Produkte
- 06/28/2017
- 1.29 MB
2712-04x Series Pneumatic Side Action Grips Data Sheet
Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.
- Produkte
- 03/22/2022
- 1.13 MB
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.
- Produkte
- 02/26/2017
- 3.76 MB