ISO » 고무 접착, 가황처리, 열가소성 수지 처리된 직물의 접착 강도 (ISO 36)

고무 접착, 가황처리, 열가소성 수지 처리된 직물의 접착 강도 (ISO 36)

ISO 36 is used for measuring the force required to separate, by stripping, two plies of fabric bonded with rubber or a rubber layer and a fabric ply bonded together. This test is used for the determination of median peak force and the adhesion strength characteristics of the product for a given rate of displacement.

This method is applicable when the ply surfaces are approximately plane or when they are in the form of a cylinder having an internal diameter greater than approximately 50 mm. It is not applicable when the ply surfaces contain sharp bends, angles or other gross irregularities that cannot be excluded when cutting out test pieces.

In principle, the test specimen is clamped in the jaws of the testing machine, ensuring the test specimen is properly gripped. A force is applied at a constant rate of displacement - tearing the specimen until fracture. The tear force is calculated from the force peaks.To record the test it is important to have a high speed intelligent test data logging rate. This is the transfer rate to the PC of 100Hz or more to capture and record all the peaks and troughs.

We use pneumatic action grips with rubber coated jaw faces for clamping of the material fitted to a tensile testing machine. While manual action grips will work, many of our users prefer the pneumatic action grips for ease of use, productivity, and better repeatability. Pneumatic action grips allow you to set a clamping pressure, while the manually operated grips depend on the operator's strength (which may not be so repeatable). We find that gripping pressure and specimen alignment are very important in these tests. Too much gripping pressure can produce premature breaks, while not enough gripping pressure can lead to specimen slippage or breaks at or near the jaws. These grips are usually fitted to either a single-column or dual-column design. Using testing software, such as the Bluehill® 2 test method, is ideal for inputting specimen details, setting the desired test control, automatically calculating the desired results and statistics, and producing a test report all in accordance with the standard.

We suggest reviewing ISO36 to fully understand the test fixture and results requirements.

문헌

6800 시리즈 프리미어 시험 시스템 브로슈어

Instron 6800 시리즈 만능 시험기는 비교할 수 없는 정확도와 신뢰성을 제공합니다. 특허 출원 중인 Operator Protect 시스템 아키텍처를 기반으로 완전히 새로운 Smart-Close Air Kit 및 충돌 완화 기능을 갖춘 6800 시리즈는 재료 시험을 그 어느 때보다 간편하고, 스마트하며, 안전하게 만들어줍니다.

  • 제품소개
  • 02/10/2020
  • 3.56 MB

2710 Series Screw Side Action Grips

Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.

  • 제품소개
  • 06/28/2017
  • 1.29 MB

2712-04x Series Pneumatic Side Action Grips Data Sheet

Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.

  • 제품소개
  • 03/22/2022
  • 1.13 MB

Bluehill Universal 브로슈어

Bluehill Universal은 직관적인 터치 인터페이스와 간소화된 워크플로우를 위해 설계된 Instron의 첨단 재료 시험 소프트웨어입니다. 사전 로드된 시험 방법, 신속한 설정을 위한 QuickTest, 향상된 데이터 내보내기, 직접적인 서비스 통신을 위한 Instron Connect를 제공합니다. Bluehill 2 및 Bluehill 3 사용자는 향상된 성능과 사용성을 위해 최신 버전으로 쉽게 업그레이드할 수 있습니다.

  • 제품소개
  • 02/26/2017
  • 4.61 MB