ASTM D1876 접착제의 박리 저항, T-박리시험

ASTM D1876 measures the comparative peel properties of adhesive bonds between flexible adherends by using a T-peel test. The test is referred to as a “T-peel” due to the shape the two flexible adherends form as they are pulled apart. Average peel strength for each specimen type and average, minimum, and maximum peeling loads for each individual specimen are the primary results of interest. Manufacturers use this standard for quality control in a wide range of industries as it is primarily intended for determining relative peel resistance between individual specimens or different types of adhesives. Direct comparison of different adhesives can only be made when specimen construction and test conditions are identical.
Materials
- Adhesives
Test Types
- Tension
- Peel, Tear, Friction
Standard
- ASTM D1876
ASTM D1876 Test Setup
For peel tests, it is critical to use a high data acquisition rate to register all peaks and troughs in the data. Insufficient bandwidth may overlook important test events and lead to artificially low peel strength values. For this reason, we recommend an Instron 6800 series test frame, which enables a data capture rate of up to 5 kHz. The ASTM D1876 standard states that the maximum specimen load should fall between 15% and 85% of the maximum frame capacity, in most cases making a single column frame (68SC) with capacity of 5 kN or less ideal. If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.
| ASTM D1876 Test Setup | |
|---|---|
|
6800 Series Universal Testing System
|
|
|
Bluehill Universal Software
|
|
|
2580 Series Load Cell
|
|
|
2712-041 (1 kN) Pneumatic Side-Action Grips
|
|
Grips
Pneumatic side action grips prevent specimen slippage by maintaining a constant clamping pressure throughout testing. They are available in capacities from 50N to 10kN, appropriate for the full range of adhesive strengths. Both advanced side action grips and pneumatic grips feature quick-change jaw faces that can be easily changed to accommodate different materials.
TIPS AND TRICKS
- When testing to ASTM D1876, the two adherends do not need to be the same material or thickness. However, if one adherend is more flexible than the other, attach the less flexible one to the moveable (top) grip.
- Bluehill Universal software comes with with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards. ASTM D1876 is included as part of the Adhesives module.
It is important to review ASTM D1876-08(2015)e1 in order to fully understand the test setup, procedure, and results requirements.
6800 시리즈 프리미어 시험기 브로셔
Instron 6800 시리즈 만능 시험기는 최고의 정확도와 신뢰성을 제공합니다. 6800 시리즈는 완전히 새로운 Smart-Close Air Kit 및 Collision Mitigation 기능이 있는 특허 출원 중인 Operator Protect 시스템 아키텍처를 기반으로 하며, 그 어느 때보다 간편하고 스마트하며 안전한 소재 시험을 가능하게 합니다.
Bluehill Universal 브로슈어
Bluehill Universal은 직관적인 터치 상호 작용과 간소화된 워크플로우를 위해 설계된 Instron의 고급 재료 시험 소프트웨어입니다. 이 소프트웨어는 사전 로드된 시험 방법, 빠른 설정을 위한 QuickTest, 향상된 데이터 내보내기, 그리고 직접적인 서비스 통신을 위한 Instron Connect를 제공합니다. Bluehill 2 및 Bluehill 3 사용자들은 향상된 성능과 사용 편의성을 위해 최신 버전으로 쉽게 업그레이드할 수 있습니다.
2712-04x Series Pneumatic Side Action Grips Data Sheet
Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.
2712-05x Series Pneumatic Side Action Grips Data Sheet (50 N and 250 N)
The Instron 2712-05x Series Pneumatic Side-Action Grips offers a versatile gripping solution for a wide range of materials. Available in both 50 and 250 N options, the grip’s robust design is ideal for round (wires),fiber (mono-filaments), and flat specimens with or without shoulder.
2710 Series Screw Side Action Grips
Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.