The Challenge

Mechanical testing of stents involves a range of different tests that encompass both static and fatigue methods. Stents are most commonly made from Nitinol wire, which must be tested to ASTM F2516 in a simple cyclic test. Another static test that is often carried out on stents is a flexural test in accordance with ASTM F2606. In addition to testing the raw material, the diamond structure of the stent body is commonly tested in fatigue at 60 Hz in position control. The entire stent body is also typically tested in radial compression as a static test, and pulsatile fatigue or cyclic fatigue as a dynamic test. Considering that such a variety of mechanical tests are required on any single stent, it is often challenging to select the appropriate test system for conducting as many tests as possible.