Pneumatic Cord and Yarn Grips. Grooved, 5 kN

CP105953 | Pneumatic Cord and Yarn Grips

Capacity: 5.0 kN (1,000 lb, 500 kg).

Incorporates a grooved channel for specimen guidance.

Temperature range: -10 °C to 80 °C (14 °F to 176 °F).

Maximum specimen diameter: 2 mm (0.08 in).

Upper and lower fittings: Type Dm (1.25 in connection with ½ in clevis pin).

Requires a rigid coupling and an Automatic Air Control Kit or Pneumatic Foot Switch

Unterlagen

Pneumatic Tire Cord Grips (CP105953)

The Instron® pneumatic tire cord grips provide a convenient method for clamping tire cord and braided wire during testing.