Inertial Peak (impact)
The first peak in a force-time or force-deflection curve obtained during an instrumented impact test. It arises from the inertia of that part of the test specimen (referred to as the contact mass) which is accelerated after the first contact with the striker (contact between specimen and striker can be temporarily lost). The peak force increases approximately linearly with increasing impact velocity, while the duration decreases. At impact velocities above 2 m/s, the duration is approximately constant but depending on the material being tested.
References
- ISO 179-2: 1997
Broschüre der Universalprüfsysteme der Serie 3400
Instron Universalprüfsysteme der Serie 3400 für Zug-, Druck-, Biege- und andere Materialeigenschaftsprüfungen.
Broschüre Serie 6800 Premier Testing Systems
Universal-Testsysteme der Instron Serie 6800 bieten unvergleichliche Genauigkeit und Zuverlässigkeit. Die 6800 Serie basiert auf einer zum Patent angemeldeten Operator-Protect-Systemarchitektur mit einem brandneuen Smart-Close Air Kit und Collision-Mitigation-Funktionen, wodurch Materialtests einfacher, intelligenter und sicherer sind als je zuvor.
Bluehill Universal Broschüre
Bluehill Universal ist die fortschrittliche Materialprüfsoftware von Instron, entwickelt für intuitive Touch-Interaktion und optimierte Arbeitsabläufe. Sie bietet vorinstallierte Prüfmethoden, QuickTest für eine schnelle Einrichtung, verbesserten Datenexport und Instron Connect für die direkte Servicekommunikation. Anwender von Bluehill 2 und Bluehill 3 können problemlos auf die neueste Version upgraden, um die Leistung und Benutzerfreundlichkeit zu verbessern.