Tensile Impact Test Method with Drop Weight Impact Tester
Tensile Impact Test at High Strain Rates
How to perform Tensile Impact test
A tensile impact test measures the toughness of polymers using an impact tester for plastic according to the ISO 8256 standard. Polymers that are too flexible or thin for a Charpy or Izod impact test generally require an uniaxial tensile impact test with a relative high strain rate.
When evaluating the elastic response of a
material, quasi-static tensile testers are used to determine most of the
mechanical properties . However, a wide variety of polymeric materials are sensitive to strain and require an impact tester for plastic that can run a tensile impact strength test at both quasi-static and high velocities.
.
The Instron impact test apparatus can reach a wide range of
impact velocities from relatively low (0.7 m/s) to very high (22m/s). Thanks to
variable impact masses, the test
velocity remains as constant as possible during the elongation of the specimen.
Instron’s impact test apparatus covers impact energies between 1 and 1,800 J.
- A dedicated tensile-impact striker
- A tensile-impact vice equipped with a piezoelectric load cell (up to 2.2 kN) or a strain-gauge sensor (up to 15 kN), a screw grip with V-shaped jaw faces and a calibrated free tensile grip (crosshead)
- A Data Acquisition System with a piezoelectric or strain-gauge channel
With the combined use of a drop weigh impact testing machine equipped with Bluehill® Impact Software, tensile impact accessories, High Speed Camera and Digital Image Correlation software, it is possible to evaluate the longitudinal strain of the specimen when impacted under tensile-Impact conditions.
Instron recommends Photron High Speed Camera Fastcam Mini Series.
Broschüre der Universalprüfsysteme der Serie 3400
Instron Universalprüfsysteme der Serie 3400 für Zug-, Druck-, Biege- und andere Materialeigenschaftsprüfungen.
Broschüre Serie 6800 Premier Testing Systems
Universal-Testsysteme der Instron Serie 6800 bieten unvergleichliche Genauigkeit und Zuverlässigkeit. Die 6800 Serie basiert auf einer zum Patent angemeldeten Operator-Protect-Systemarchitektur mit einem brandneuen Smart-Close Air Kit und Collision-Mitigation-Funktionen, wodurch Materialtests einfacher, intelligenter und sicherer sind als je zuvor.
Bluehill Universal Broschüre
Bluehill Universal ist die fortschrittliche Materialprüfsoftware von Instron, entwickelt für intuitive Touch-Interaktion und optimierte Arbeitsabläufe. Sie bietet vorinstallierte Prüfmethoden, QuickTest für eine schnelle Einrichtung, verbesserten Datenexport und Instron Connect für die direkte Servicekommunikation. Anwender von Bluehill 2 und Bluehill 3 können problemlos auf die neueste Version upgraden, um die Leistung und Benutzerfreundlichkeit zu verbessern.