Furnace Testing
For Fatigue Testing Systems
Furnace Testing
Our standard furnaces and load string assemblies for fatigue testing systems allow for testing up to 1000°C in air. Our engineered solutions group is also able to develop solutions to meet higher temperature requirements and additional furnace dimensions.
1000°C Three-Zone Split Tube Furnace
Catalog No. 3117-200
Catalog No. 3117-200
Designed for low cycle fatigue testing, this three-zone split tube furnace features durable embedded heating elements, high efficiency insulation, and a side entry extensometer port.
| Related Accessories | |||
| Description | Catalog No. | ||
| Furnace Controller and Software | 3117-301 3117-302 |
||
Hydraulic Reverse-Stress Pull Rods
Catalog No. 3117-501
Catalog No. 3117-501
Designed for elevated temperature low cycle fatigue applications in addition to hot tensile testing and other reverse axial stress applications.
| Specifications | |||
| Maximum Pressure | 130 bar | ||
| Maximum Operating Temperature | 1050°C (1922°F) | ||
| Related Accessories | |||
| Description | Catalog No. | ||
| Electrically Operated Pump | 3117-503 | ||