Proportional Limit

The proportional limit is the point on a stress-strain curve where the linear, elastic deformation region transitions into a non-linear, plastic deformation region. In other words, the proportional limit determines the greatest stress that is directly proportional to strain. The transition point can be calculated by a specified percent change in slope. Because the proportional limit is not required by many test standards,  it is often used for educational purposes rather than in practice by the materials testing industry.

How is Proportional Limit Different from Elastic Limit?

The elastic limit is the greatest stress that can be applied to a material without causing plastic (permanent) deformation. For many materials the elastic limit is equivalent or nearly equivalent to the proportional limit. For other materials, such as elastomers, the stress-strain relationship is non-linear and the material will still be within its elastic region long after it has passed through its proportional limit. The elastic limit is essentially a theoretical value that is difficult to determine using a universal testing machine, and for this reason is used mainly for educational purposes rather than in practice by the materials testing industry.

How is Proportional Limit Different from Yield Strength?

Similar to the elastic limit, the yield strength of a material can also occur beyond the material’s proportional limit. Unlike the elastic limit, the yield strength on a stress-strain curve has been defined by ASTM and ISO test standards. Depending on the material’s stress-strain behavior at yield, a preferred yield calculation is specified by the chosen standard. For instance, metals test standards (ASTM E8 or ISO 6892) have standardized a 0.2% offset yield, which allows the metals industry to objectively evaluate different metals against each other. The stress-strain curve below displays the difference between the proportional limit (4% change in slope) and the 0.2% offset yield point in a metals test.

the difference between the proportional limit example
Related Content

3400 Series – โซลูชันการทดสอบราคาประหยัด

ระบบทดสอบอเนกประสงค์ Instron 3400 ซีรีส์สำหรับการทดสอบแรงดึง แรงอัด การดัดงอ และคุณสมบัติอื่น ๆ ของวัสดุ

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability