Our Solution

With an array of implant sizes and geometries, angled dental implants can be mounted into an Instron® dental variable angle fixture for testing. The fixture ensures that the mounting neither over constrains the implant nor generates large lateral forces that can damage the load cell or the testing machine. As with straight dental implants, pre-angled dental implants can also be tested in an aqueous environment, if corrosion fatigue is expected to occur. The fixture can be mounted in a fluid bath to test the implant in saline solution, or other physiological medium, while the temperature is maintained at 37°C.