Transverse Averaging Extensometer for "r" Value on Sheet Metal
Catalog no. 2640-010
2640-010 | Transverse Averaging Extensometer
Transverse Averaging Extensometer with single channel output for attachment to thin rigid specimens, 0.3 mm to 4 mm thick.
Accepts specimens from 10 mm to 20 mm wide and from 15 mm to 25 mm wide. Suitable for ´r´ and ´n´ testing on sheet metals.
Requires suitable axial extensometer of 50 mm gauge length minimum for ´r´ value determination. Requires single strain conditioner.
Temperature Range: -80 °C to +100 °C
2640 Series Averaging Transverse Extensometer | 2640-010
The 2640 series averaging transverse extensometer is designed to measure average transverse gauge length and strain with a single output channel.