Necking

The term "necking" is used in engineering and materials sciences to describe the localized reduction of cross-sectional area of a specimen under tensile load. Necking occurs when an instability in the material causes its cross-section to decrease by a greater proportion than the strain hardens when undergoing tensile deformation. If the material begins to harden by a smaller proportion than the decrease in cross-sectional area, strain concentrates at the location of highest stress or lowest hardness. The greater the local strain, the greater the local decrease in cross-sectional area, which in turn causes even more concentration of strain, leading to an instability that causes the formation of a neck. Necking behavior is disregarded in calculating engineering stress but is taken into account in determining true stress.

specimen necking

 

Related Content

Brochura do Bluehill Universal

O Bluehill Universal é o software de teste de materiais avançado da Instron, projetado para interação tátil intuitiva e fluxos de trabalho simplificados. Ele oferece métodos de teste pré-carregados, QuickTest para configuração rápida, exportação de dados aprimorada e Instron Connect para comunicação direta com o serviço. Os usuários do Bluehill 2 e do Bluehill 3 podem atualizar facilmente para a versão mais recente para melhor desempenho e usabilidade

Série 3400 – Soluções de teste acessíveis

Sistemas de teste universal Instron série 3400 para testes de tração, compressão, curvatura e outros testes de propriedades de materiais.

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.