ASTM D413 Rubber Property-Adhesion to Flexible Substrate
ASTM D413 method is used to determine the adhesion strength required to separate a rubber layer from a flexible substrate such as a fabric, fiber, or sheet metal. The standard defines three test procedures: Type A - 180°peel, Type B - 90°peel, and Type C - 90° peel for ring specimens. The adhered rubber is pulled from the flexible substrate to measure the adhesion strength, also known as the average force divided by the specimen width, over a distance of at least 100mm at a constant rate.
The challenges of testing to this standard are:
- Maintaining a 90°and 180° angle throughout the test
- Bandwidth and data rate to capture peaks and troughs
Instron's Solution:
- Maintaining a 90° angle throughout the test – The 90° peel fixture is able to maintain this angle by using a low force sliding table that is adjusted throughout the test. The fixture consists of a bearing mounted table, which is linked to the test system via a cable and pulley, as well as anchored on the back by a dampening coil spring. As the crosshead is driven in the tensile direction, the cable pulls the table to maintain a constant 90° angle peel, and the coil spring keeps the table from reacting to inertia caused by load peaks and troughs. This fixture is adaptable for both single and dual column frames.
- Maintaining a 180°angle throughout the test - The pneumatic side action grips are able to maintain constant gripping pressure throughout the test, which ensures repeatability. The advanced screw side-action grips can also provide an adequate and affordable solution for this test. Both grips employ a patented "quick-change" jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials.
- Bandwidth and data rate to capture peaks and troughs – Instron’s 6800 Series frames have multiple data bandwidth options which provide flexibility especially when acquiring fast changing data on events that occur rapidly. Instron’s 6800 Series frames also enables data capture of up to 5 kHz to ensure that all fast changing events are captured. If bandwidth and data capture rate are too low, this can lead to missed peaks and troughs, resulting in lower average strength values.
90° Angle Peel Fixture (2820-035)
Both the 90° peel test fixture and the variable angle peel test fixture consist of a bearing-mounted sled that is linked to the testing machine’s crosshead by a cable and pulley system.
- Produtos
- 10/10/2018
- 590.73 KB
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Produtos
- 02/10/2020
- 1.93 MB
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability
- Produtos
- 02/26/2017
- 3.76 MB
2710 Series Screw Side Action Grips
Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.
- Produtos
- 06/28/2017
- 1.29 MB