Instron

Productos » Accesorios de ensayo » Extensómetros » Transverse Clip-on Extensometers » Transverse Extensometer, range +/- 0.1 in

Transverse Extensometer, range +/- 0.1 in

W-E404-C | Transverse / Diametral Strain Gauge Extensometer

+/- 0.10 in travel

For general purpose transverse or diametral strain measurement
on axially loaded specimens. Used for measurement of Poisson's ratio,
on anisotropic materials like many composites and similar applications.

Specifications:

  • Specimen Width or Diameter: 0 to 25 mm (0 to 1.0 in)
  • Travel: +/- 0.10 in.
  • Temperature Range: -40°C to 100°C (-40°F to 210°F)
  • Standard Instron 25 pin connector.
Literatura

W-E404 Series Transverse Extensometers

W-E404 Series Transverse Extensometers are designed for measuring transverse displacements. They are self-supporting on the test specimen and will work on any width or diameter specimen from 0 to 25 mm(1 in).

  • Productos
  • 12/10/2007
  • 452.3 KB

Tabla de especificaciones