Creep
Deformation that occurs over a period of time when a material is subjected to constant stress at constant temperature. In metals, creep usually occurs only at elevated temperatures. Creep at room temperature is more common in plastic materials and is called cold flow or deformation under load. Data obtained in a creep test usually is presented as a plot of creep vs. time with stress and temperature constant. Slope of the curve is creep rate and end point of the curve is time for rupture. As indicated in the accompanying diagram, the creep of a material can be divided into three stages. First stage, or primary creep, starts at a rapid rate and slows with time. Second stage (secondary) creep has a relatively uniform rate. Third stage (tertiary) creep has an accelerating creep rate and terminates by failure of material at time for rupture.
Serie 3400 – Soluciones de ensayo asequibles
Sistemas de ensayo universales Instron Serie 3400 para ensayos de tracción, compresión, flexión y otras propiedades de los materiales.
Catálogo de sistemas de ensayo Serie 6800 Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Contáctenos
Por favor rellene el siguiente formulario y estaremos encantados de contactar con Ud. Si su pregunta está relacionada con una solicitud de servicio, por favor complete y envíe este formulario. Nuestro tiempo de respuesta de una solicitud en línea está dentro de 1-2 días laborales. Si requiere de una respuesta más rápida, por favor llame al +34 935 947 560