Risorse » Glossario dei termini relativi alle prove sui materiali » Strain Hardening Exponent

Esponente di Incrudimento

Measure of increase in hardness and strength caused by plastic deformation. It is related to true stress and true strain by the equation:
s = s0d h where s is true stress, s0 is true stress at unit strain, d is true strain and h is strain hardening exponent.