ISO » ISO 14126 In-Plane Compressive Properties of Fiber-Reinforced Plastic Composites

ISO 14126 In-Plane Compressive Properties of Fiber-Reinforced Plastic Composites

ISO 14126 describes the methodology for determining the in-plane compressive properties of fiber-reinforced plastic composites. The standard describes two different methods for evaluating the properties:

  • Method 1: provides for shear loading of the specimen
  • Method 2: provides for end loading or mixed loading of the specimen

Ultimately, these two methods require two different test fixtures. The more common method of the two is Method 1, which uses a Celanese-type fixture (shown at right). Also, in both methods, the specimen gauge length is completely unsupported.

For the Method 1 test, the specimen is supported in the fixture and compressed, using hardened-steel compression anvils, along its major axis at constant rate of displacement until the specimen fractures. Because of the typically high forces that are recorded during this test, we usually recommend a dual-column electromechanical testing system.

Finally, accurate strain measurement is required for making measurements such as compressive modulus or compressive failure strain. Therefore, either a suitable extensometer or bonded resistance strain gauges are required for measuring axial strain throughout the test.

Literature

2810-400 Series Flexure Fixture

The Instron® 2810 Series Flexure Fixture allows a variety of flexural tests to be performed, including determination of flexural modulus, flexural strength, and flexural yield strength.

  • Prodotti
  • 05/12/2021
  • 692.27 KB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Prodotti
  • 02/10/2020
  • 4.15 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • Prodotti
  • 06/27/2022
  • 2.69 MB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Prodotti
  • 02/26/2017
  • 3.76 MB

2630 Series Strain Gauge Extensometers

The 2630-100 series of extensometers offers speed of attachment and ease-of-use. The light-weight, rugged cross-brace design eliminates errors caused by physical distortion, while built-in protection ensures that damage is not caused by over-extension.

  • Prodotti
  • 06/03/2013
  • 551.73 KB