1000°C Three-Zone Split Furnace for Low Cycle Fatigue Testing

Catalog no. (Various)

Three-zone Split Furnace
Three-zone Split Furnace W8518HPjpg FurnaceAccessoriesPjpg Furnaces W754XXP2jpg

1000°C Three-Zone Split Furnace for Low Cycle Fatigue Testing

Features:

90mm bore diameter, 358mm overall height (furnace only)

Three-zone split furnace configuration with durable embedded heating elements

1000 °C (1832 °F) nominal maximum specimen temperature (dependent on load string configuration)

300 - 600 °C (572 - 1112 °F) nominal minimum specimen temperature (dependent on load string configuration and test conditions)

High efficiency insulation (refractory ceramic fibre free)

Extensometer cut-out, full width, 76 mm high

Extensometer slot 40 mm high x 15 mm wide

Nominal power rating 3kW

Includes side port insulation plug for blanking extensometer slot.

Requires temperature controller with thermocouples, support brackets, and top/bottom insulating port plugs (not included)

For Use With

  • Axial Extensometer; 12.5mm Gauge Length +20% -10% Capacity
  • Axial Extensometer; 12.5mm Gauge Length, +20% / -10% Capacity
  • Strain Gauge Extensometer; 25mm Gauge Length, +10% -5% Capacity
  • High-Temp Extensometer; 25mm Gauge Length, +10% -5% Capacity
  • Leaf Spring Mounting for 2632-054, -055, 056 and -057 Extensometers