Transverse Extensometer, range +/- 2.5 mm

Catalog no. W-E404-F

W-E404-F | Transverse / Diametral Strain Gauge Extensometer

+/- 2.5 mm travel

For general purpose transverse or diametral strain measurement
on axially loaded specimens. Used for measurement of Poisson's ratio
on anisotropic materials like many composites and similar applications.

Specifications:

  • Specimen Width or Diameter: 0 to 25 mm (0 to 1.0 in)
  • Travel: +/- 2.5 mm
  • Temperature Range: -40°C to 100°C (-40°F to 210°F)
  • Standard Instron 25 pin connector.
Literature

W-E404 Series Transverse Extensometers

W-E404 Series Transverse Extensometers are designed for measuring transverse displacements. They are self-supporting on the test specimen and will work on any width or diameter specimen from 0 to 25 mm(1 in).