Instron

Flexure Fixture, Fatigue 3 Point

Catalog no. 2810-181

2810-182_P
2810-182_P

Flexure Fixture, Fatigue 3 Point 2810-181

Fatigue Rated 3 Point Bend Fixture, 100 kN (22 kip) Dynamic Capacity, With 25mm (1.0 in) Diameter Rollers

  • Adjustable lower span from 30 to 250mm (1.18 to 9.8 in)
  • Maximum specimen width is 50mm (2 in)
  • Mechanical interface: M30 x 2 right hand female threads
  • Anti-rotation is incorporated in the design

Includes: One upper roller, 25 mm (0.97 in) Diameter

Requires: fatigue rated adapters

 

 

Specifications
Accessory Height 270 mm (10.54 in)
Accessory Weight 20 kg (44 lb)
Accessory Width 352 mm (14 in)
Anvil Diameter 25 mm (0.98 in)
Capacity 100 kN (22,500 lbf)
Loading Span 0 mm (0 in)
Lower Fitting M30 RH (Type If)
Specimen Width 0 - 50 mm (0 - 2 in)
Static or Fatigue Rated Fatigue
Support Span 10 - 250 mm (0.39 - 10 in)
Temperature Rating -100 to +350 °C (-148 to +660 °F)
Upper Effective Length 90 mm (3.54 in)
Upper Fitting M30 RH (Type If)
Add-Ons
Literature
For Use With