Compact Tension Fixtures for 50mm Wide Compact Tension Specimens

Catalog no. 2750-120

2750-120 | Compact Tension Fixtures for 50mm wide Compact Tension Specimens

Fracture Mechanics Fixtures for 50 mm wide compact tension specimen.

Rated capacity: ±250kN Dynamic, 500 kN Static

Requires: fatigue rated adapters. Mechanical interface M48 x 2 right hand female thread.

(1 Pair)

Specifications
Capacity ±250 dynamic, 500 static kN (±56,200 dynamic, 112,000 static lbf)
Specimen Width 50 mm (1.97 in)
Testing Standards ASTM E399, ASTM E647, ASTM E813, ASTM E1290, BS7448