Catalog no. 2780-119

2780-119 | Compact Tension Fixtures for 25mm Thick Compact Tension Specimens

Designed in accordance with international standards such as ASTM E399, E647 & E1820

Rated Capacity: ±50kN Dynamic, 100kN Static

Temperature Range: -50 to 315°C

Includes:

  • Piston rod extender to reduce the minimum daylight between Loadcell and ±75mm actuator at mid-stroke to allow compact tension fixtures to touch (Quantity 1).
  • Fatigue Rated Adaptors. M30 x2 right hand male to male stud with preloading wedge washers (Quantity 2)

Note: Requires 2780-120 for use with a standard 3119-600 Series Chamber

Specifications
Capacity ±50 dynamic, 100 static kN (±11,500 dynamic, 22,500 static lbf)
Specimen Width 25 mm (0.98 in)
Testing Standards ASTM E399, ASTM E647, ASTM E1820