Specimen Preparation Devices

Products » Testing Accessories » Specimen Preparation Devices

Proper preparation, accurate measurement, and reliable marking of specimens are critical for accurate material characterization.

Micrometer measurement system
Micrometer measurement system Vertically mounted probe with automatic measurement system Handheld automatic caliper measurement system

Automatic Specimen Measurement Devices

Instron® offers a variety of specimen measurement devices capable of sending the digital measurement captured on the device directly to Bluehill® Universal testing software, eliminating manual data entry for specimen measurements.

Description Range Resolution Catalog Number
Micrometer Measurement System
Includes micrometer with ratchet, digital indicator, stand, footswitch, USB interface, and connecting cables
0–25.4 mm
0–1.0 in
0.001 mm
0.00005 in
2850-007
Handheld Automatic Caliper Measurement System
Includes a handheld caliper with digital indicator, carbide tips, footswitch, USB interface, and connecting cables
0–150 mm
0–6 in
0.01 mm
0.0005 in
2850-005
Vertically Mounted Probe Measurement System
Includes vertically mounted gauge probe with indicator, stand, tip set, footswitch, USB interface, and connecting cables
0–25 mm
0–1.0 in
0.001 mm
0.00005 in
2850-003
Interface Box
Interface box to connect two specimen measurement devices (micrometers, calipers, digital indicators, etc.) to a PC
2850-015

More Info

Manual gauge point punch
Manual gauge point punch Gauge punch Manual gauge point punch in use

Manual Gauge Point Punches

Gauge point punches are used to punch mark a metallic specimen with a set gauge length before testing so that specimen elongation can be measured either during or after the test. Manual punches are available for a range of different gauge lengths.

Gauge Length Catalog Number
0.5 in W-6718
Combination Gauge Point Punch: 1 in and 2 in W-6771
Combination Gauge Point Punch: 25 mm and 50 mm W-6771-B
1.4 in W-6719
8 in W-6714
Extra Punch Points — Set of 2
Suitable for 1 in, 1.4 in, 2 in, 25 mm, and 50 mm gauge point punches
W-6709
Replacement Punch Points — Set of 2
Suitable for 8 in gauge point punch
W-6704

Contact Us for More Details

Specimen punching machine
Specimen punching machine Punched specimens Punched material sheet

Punching Machines — Specimen Preparation

These machines are developed to obtain specimens by punching, using hollow dies of different sizes and contours. Several hundreds of dies can be created by interchangeable socket punches with different profiles and size according to the standards and the application needs. Dies are made of steel with hand-finished cutting edges and can be provided with an ejector for easy removal of the specimen after punching.

Create specimens for testing to the following standards: ISO 2818, ISO 179, ISO 180, ISO 8256, ASTM 6110, ASTM D256, ASTM D412, ASTM D638, and DIN 53453.

Description Catalog Number
Manual Version C-6051-000
Pneumatic Version

  • Punching Stroke: 18 mm (0.71 in)
  • Maximum Punching Force: 40 kN
C-6054-000

Contact Us for More Details

Notching machine for specimen preparation
Notching machine for specimen preparation Notching machine for specimen preparation

Notching Machines — Specimen Preparation

Notching machines are designed to notch specimens for impact resilience according to Izod, Charpy, and tensile impact methods. These instruments use a linear knife-cutting technique to avoid overheating and consequent stresses during the specimen's notching operations. Therefore, accurate notch preparation is guaranteed.

Create specimens for testing to the following standards: ISO 2818, ISO 179, ISO 180, ISO 8256, ASTM 6110, ASTM D256, and DIN 53453.

Description Catalog Number
Manual Version

  • Notch up to 7 specimens (4mm thickness) in a single operation
C-6897-000
Motorized Version

  • Notch up to 7 specimens (4mm thickness) in a single operation
  • Micrometric head with digital readout of cut depth (resolution 0.001 mm)
  • Speed variator
C-6898-000
Automatic Version

  • Notch 50 specimens in a single cycle for high productivity
  • Adjustable cutting speed for more sensitive materials
  • Store key parameters for later use
  • Knife cooling system included
  • Optional slicing device
  • Optional double notch loader
C-6899-000

Contact Us for More Details