Instron
  • Back
  • Home
  • Products
    Testing Systems
    Universal Testing Systems
    Structural Durability
    Automated Testing Systems
    Dynamic and Fatigue Testing Systems
    Crash Simulation
    Torsion Testers
    Rheometers & Melt Flow Testers
    Impact Drop Towers & Pendulums
    HDT & Vicat
    Out of Production Systems
    Accessories
    Software
    Load Cells
    Peel, Friction, Puncture
    Environmental Chambers and Furnaces
    Tensile Grips
    Flex Fixtures
    Biomedical Testing Accessories
    Electronics Testing Accessories
    Extensometers
    Compression Platens
    Battery Testing Accessories
    Composite Testing Fixtures
    Specimen Measuring and Preparation
    All Accessories
  • Industry Solutions
    ASTM Standards ISO Standards Other Standards
    Industries
    Automotive
    Batteries
    Biomedical
    Electronics
    Materials
    Composites
    Metals
    Plastics
  • Service and Support
    Instron Remote Technical Support Product Life Cycle Service Success Stories Training
    Services
    Calibration and Verification
    Instron Implementation Assistance
    Installation & Relocation
    Tech Support
    FAQs
    Software Update Services
    Resources
    Manuals
    Serial Number Locator
  • Our Company
    Careers Press Room Subscribe to Our Newsletters
    About Us
    Our History
    Locations
    Accreditations & Certificates
    Resources
    Glossary
    Test Types
    Literature Library
    Case Studies
    News
    Blog
    Webinars
    Events
    Privacy & Terms
    Accessibility
    Cookie Notice
    Export Control
    Data Privacy Notice GDPR
    Privacy Notice
    Terms & Conditions
    Terms of Use
  • Contact Us
  • Global Site
Testing Solutions » Others » BSS 7260 Post-Impact

BSS 7260 Post-Impact Compressive Strength of Composite Laminates

Standard

  • ASTM D7137
  • JIS K7089
  • Boeing® BSS 7260

Materials

  • Composites

Business Sector

  • Aerospace and Suppliers
  • Contract Testing Services

Test Types

  • Compression

Specimen

  • Rectangular
Contact usView Accessories Catalog
Boeing BSS Compression after impact test, Instron
  • Boeing BSS Compression after impact test, Instron
  • Description
  • Contact Us

A compression after impact (CAI) test is used to measure the residual strength of composite laminates after being damaged by an impact. Such damage can be caused by dropping tools on a laminate or by flying debris. Even if the impact does not result in visible damage, the compressive strength of the composite can be compromised.

The CAI test method and the associated test fixture are outlined in Boeing® Specification BSS 7260. This post-impact compression test is targeted for carbon and aramid fiber reinforced plastic (CFRP) composite laminates. It is widely used to assess the relative performance of composite laminates with different fiber matrix combinations.

Before testing the compressive strength of the composite, we simulated impact damage by applying a specific energy with an instrumented impact tester; alternatively, you could use the manual drop weight approach.

Next, we used a floor model electromechanical universal tester equipped with our Boeing CAI Test Fixture and Bluehill® Software to apply the compressive force. The post-impact test fixture incorporates adjustable side plates to accommodate for both variations in thickness and overall dimension. It is designed to prevent specimen buckling while the specimen is end-loaded to failure.

Your Email Address

Please enter your email address. Email addresses must contain the @ symbol. Email addresses can only contain letters, numbers and the following special characters: . ! # $ % & ' * + - / = ? ^ _ ` { | } ~ Email address domains can only contain letters, numbers, dots (.) and hyphens (-).

Your Message

750 Character Max Please enter your message. Email addresses can only contain letters, numbers and the following special characters: . ! # $ % & ' * + - / = ? ^ _ ` { | } ~
Next Checking to see if you are a returning visitor…

Welcome back!

Your Contact Information

Please enter your first name. Please use letters and numbers only.
Please enter your last name. Please use letters and numbers only.
Please select your country.
Please enter your company. Please use letters and numbers only.
Please enter your address. Please use letters and numbers only.
Please enter your address line 2. Please use letters and numbers only.
Please enter your address line 3. Please use letters and numbers only.
Please enter your county. Please use letters and numbers only.
Please enter your city. Please use letters and numbers only.
Please select your state/province.
Please enter your ZIP/Postal Code. Please use numbers only
Please enter your telephone number. Please use numbers only

Please confirm that you agree with our privacy and cookies policy to submit this form.

I agree to the terms & conditions of Instron's Privacy and Cookies Policy.

Subscribe to Instron News!
Check this box to receive pertinent commercial email from Instron focusing on products, upcoming events, and more!

Please choose a subscription option One or more required fields are empty, complete the form to continue. One or more fields contain formatting errors, fix the errors to continue. You must agree to Instron's Privacy Policy in order to continue.

Please Select Your Preferred Region

Dismiss Region Selector

Americas

  • North America
  • Brasil
  • South America

All Other Countries

  • Global Site

Europe

  • France
  • Deutschland
  • Italia
  • Polska
  • España
  • United Kingdom

Asia Pacific

  • 中国
  • India
  • 日本
  • 대한민국
  • 台灣
  • ประเทศไทย
Instron Logo White
CONTACT INFORMATION

825 University Ave
Norwood, MA,
02062-2643, US

Sales: +1 800 564 8378

Service: +1 800 473 7838

General: +1 800 877 6674

HELPFUL LINKS
  • Testing Systems
  • Software
  • Accessories
  • Catalog
  • Careers
  • News
  • Testing Solutions
  • Case Studies
  • Webinars
  • Glossary
  • Library
  • Events
Policies / Legal
  • Privacy and Cookies Policy
  • Terms of Use
  • Accessibility
  • Export Control
  • Data Notice GDPR
CONNECT WITH US
SIGN UP FOR OUR NEWSLETTER
EMAIL ADDRESS
© Illinois Tool Works Inc. All rights reserved.
[email protected]
  • Privacy and Cookies Policy
  • Terms of Use
  • Accessibility
  • Export Control
  • Data Notice GDPR