Understanding Strain Rate to ISO 6892-1 and ASTM E8

Strain rate control is one of the most misunderstood parts of common metals testing standards such as ISO 6892-1 and ASTM E8. This video breaks down what strain rate control is, why it is important, how can you implement it, and some challenges that may occur.

The Definitive Guide to Metals Tensile Testing to ASTM E8 and ASTM A370

ASTM E8/E8M and ASTM A370 are the most common test methods for determining the tensile properties of metallic materials.

Bluehill® Universal과 통합된 자동 시편 측정 장치

자동 시편 측정 장치(ASMD)는 수동 데이터 입력 및 계산 오류를 제거하여 시편 준비를 간소화하고, 빠르고 정확한 폭 및 두께 측정값을 시험 워크플로우에 직접 제공합니다.

Instron Safety: How To Use a Tensile and Compression Testing System Safely

Vipul In this video, we offer quick tips on how to safely use an Instron® universal testing system. For additional safety information, visit our manuals section to read your Instron system manual, or contact your local service representative.

AT3 Automated Film Tensile Testing to ASTM D882

The Instron® TestMaster AT3 Automated Testing System uses an innovative three-axis design for automatic tensile testing of thin films. Normal tensile testing of thin films can prove challenging, but the versatile AT3 makes it easy, improving repeatability, safety, and efficiency by automating everything from measurement to specimen handling and removal.