ISO » ISO 1926 Rigid Cellular Plastics Tensile Properties

ISO 1926 Rigid Cellular Plastics Tensile Properties

ISO 1926 method determines the tensile and deformation properties of rigid cellular materials when extended at a constant rate of displacement until failure. These properties include tensile strength and elongation at break.

The challenges:

  • Specimen gripping
  • Repeatable strain measurements
  • Reporting test results in compliance with the standard

 

Our solution:

  • Specimen gripping – Gripping options include pneumatic side action grips and advanced screw action grips. Pneumatic side action grips provide a constant clamping force to ensure no slippage occurs and ensures repeatable results.
  • Repeatable strain measurements – Advanced strain solutions include non-contacting extensometers, such as the Advanced Video Extensometer (AVE2) and automatic contacting extensometers, such as the AutoX750. These solutions require little influence from the operator, resulting in improved repeatability. Contacting long travel extensometers also meet the measurement accuracy requirements of the standard.
  • Reporting test results in compliance with the standard – Bluehill® Universal testing software offers advanced methods that are available with pre-configured calculations to ensure compliance with the standard report requirements.

 

It is important to review ISO 1926 to fully understand the test setup, procedure, and results requirements.

Literature

AVE 2 Non-Contacting Video Extensometer

The second generation Advanced Video Extensometer (AVE 2) utilizes patented measurement technology in the fastest, most accurate non-contacting strain measurement device commercially available.

  • Produtos
  • 01/26/2018
  • 1.4 MB

Automatic Contacting Extensometer – Model AutoX 750

The AutoX 750 is a high-resolution, long-travel automatic contacting extensometer. It can be mounted onto any electromechanical 3300, 3400, 5500, 5900, or 6800 Series tabletop or floor model system as well as LX, DX, HDX, and KPX static hydraulic testing systems. It is well suited for applications involving plastics, metals, biomedical, composites, elastomers, and more. The AutoX has a maximum travel of 750 mm and accuracy of ± 1 µm.

  • Produtos
  • 08/15/2013
  • 1.29 MB

2603-080 Long Travel Extensometer

The Instron model XL (long travel) extensometer is a precise device for measuring strain in highly extensible materials such as elastomers, semi-rigid plastics, and films.

  • Produtos
  • 10/23/2018
  • 478.7 KB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Produtos
  • 02/26/2017
  • 3.76 MB

2712-04x Series Pneumatic Side Action Grips Data Sheet

Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.

  • Produtos
  • 03/22/2022
  • 1.13 MB

2710 Series Screw Side Action Grips

Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.

  • Produtos
  • 06/28/2017
  • 1.29 MB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Produtos
  • 02/10/2020
  • 8.35 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • Produtos
  • 06/27/2022
  • 4.88 MB

Plastics Testing Solutions Brochure

The Plastics Testing Solutions brochure is a 40-page, applications-focused, and standards-based brochure. Important standards such as ISO 527-1, -2, -3, ISO 11443, ISO 75, ASTM D638, ASTM D3835, are covered in a detailed testing challenge and solution format. The brochure addresses the most prominent and widely-used standards in the materials testing industry for plastics. Test types such as Impact, Rheology, Thermo-Mechanical, Specimen Preparation, Mechanical Testing, Dynamic/Fatigue, and Hardness are described in great detail.

  • Applications
  • 04/12/2024
  • 12.48 MB