Finden Sie die Informationen, die Sie benötigen, an einem zentralen Ort. Die Literaturbibliothek von Instron umfasst Broschüren, E-Guides, Datenblätter, Produkthandbücher, Whitepapers und mehr und deckt unser gesamtes Sortiment an Materialprüfsystemen, Software und Zubehör ab. Ganz gleich, ob Sie Systeme vergleichen, technische Spezifikationen nachschlagen oder Best Practices für eine bestimmte Prüfung erkunden möchten – unsere Literaturbibliothek bietet Ihnen alle nötigen Informationen.
Nutzen Sie die Suchleiste, um schnell ein bestimmtes Produkt, Dokument oder Thema zu finden.

Ball Burst Test in Accordance with ASTM D 6797
Four different fabric samples were tested using a ball burst fixture in accordance with ASTM D 6797 to measure the burst strength of each and compare values between samples. The test was used to investigate the effect of different chemical treatments on the mechanical properties of the fabric.
Anwendungen 03/02/2006 697.32 KB

ASTM D 882 – Tensile Testing of Thin Plastic Sheeting
Tensile testing of thin plastic sheeting in accordance with ASTM D 882 is a common testing requirement for many Instron customers. Gripping of these delicate specimens is the prevalent challenge in most tests. The gripping technique must prevent slipping of the material at high loads but not tear into the material and cause premature specimen failure.
Anwendungen 02/22/2006 126.55 KB

Flexural Strength of Coated Fabrics Using the Miniature 3-Point Bend Fixture
A manufacturer of coated fabrics is interested in evaluating the effect of a particular coating on the flexural properties of fabric material. Four different coated fabric samples were delivered to the Instron® demonstration laboratory for evaluation.All testing was conducted in accordance with ASTM D 790.
Anwendungen 02/22/2006 964.06 KB

Tensile Testing of Textile Fabrics in Accordance with ASTM D5034
Tensile testing on textile fabrics used in the automotive industry using a grab test in accordance with ASTM D 5034.
Anwendungen 02/22/2006 651.64 KB

Puncture Tests On Plastic Containers
Application Report to briefly assess the ability of the HandHeld Mechanical Tester to perform puncture tests on disposable plastic containers. This was done quickly, without any special fixturing, for demonstration purposes only. – POD_AR_Puncture_OO1A_0902
Anwendungen 02/21/2006 610.61 KB

Elastomer-Prüfsystem MHF
Anwendungen 01/31/2006 611.73 KB

Evaluation of Tofu Firmness
Recent studies have shown a relationship between mechanical testing of food, called texture profile analysis (TPA), and the texture of food. A compression method and indentation method were used to differentiate between three varieties of tofu.
Anwendungen 01/27/2006 500.82 KB

Stossdaempfer Prüfmaschine
Stossdämpfer-Prüfmaschine Typ MSP.
System zum Prüfen und Bewerten von Werkstoffverhalten und
charakteristischen Kennwerten von unterschiedlichsten Stoßdämpfertypen (z.B. Einrohr-/ Zweirohr-Dämpfern, Sitz-, Lenkungs- und Pralldämpfern etc.)
Produkte 01/12/2006 0 B

Hydropuls Shock Absorber Test Machines
Shock Absorber Test Machines Type MSP for Damper Testing.
They are conceived to analyse and assess accurately and reliably the material properties and characteristic of all kind of damper types (e.g. single/ twin-tube shock absorbers, seat and steering dampers, metallic impactors etc.)
Produkte 01/12/2006 1.04 MB