ASTM » ASTM D885 Industrial Filament Yarns Made from Manufactured Organic-Based Fibers

ASTM D885 Tire Cord Tensile Test

This standard details the testing of fibers and cords made specifically for use in the manufacture of pneumatic tires. This standard may be applied to similar yarns and cords used for reinforcing other rubber goods and for other industrial applications. The result of this test is a determination of tensile strength of the cord being tested.

Gripping of the specimens can prove a challenge, as the cords tested with this standard are designed to be very high strength. Instron’s 2714-010 pneumatic cord and yarn grips are designed specifically for this application, and will allow specimens to be tested without slippage.

The challenges of testing to this standard are:

  • Specimen gripping

Instron's Solution:

  • Instron pneumatic tire cord grips are designed specifically for testing high strength tire cord, and are able to grip securely while maintaining high throughput

It is important to review ASTM D885-07 to fully understand the test setup, procedure, and results requirements.

Literature

Pneumatic Tire Cord Grips (CP105953)

The Instron® pneumatic tire cord grips provide a convenient method for clamping tire cord and braided wire during testing.

  • Produkte
  • 08/14/2013
  • 599.82 KB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Produkte
  • 02/10/2020
  • 4.15 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • Produkte
  • 06/27/2022
  • 2.69 MB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Produkte
  • 02/26/2017
  • 3.76 MB