ISO/TS 11405 Tensile Adhesion and Bond Strength of Dental Materials and Adhesives
Tensile adhesion and bond strength are important parameters in determining the performance of bonding materials in restorative dentistry. Although these particular types of test do not predict clinical behavior, they help scientists and researchers understand materials in a controlled laboratory environment.
ISO/TS 11405 'Dental materials - Testing of adhesion to tooth structure' helps to establish laboratory guidelines to evaluating both tensile and shear bond strength.
For a successful mechanical test of tensile bond strength, specimen alignment is critical during mounting of the specimen and as the test progresses.
Our tensile adhesion fixture for dental materials can be mounted to either a 5900 or 3300 Electromechanical Testing Machine or an ElectroPuls™ Dynamic Test Instrument. The fixture contains the necessary features to avoid uneven stress distribution upon the specimen during loading. A specimen preparation accessory helps to ensure correct alignment of the material during the setup of a test.
We recommend that you review ISO/TS 11405 to fully understand its requirements.
Interested in other types of test for dental materials or dental implants? We have a variety of solutions for testing of dental materials and implants.
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Produkte
- 02/10/2020
- 4.15 MB
3400 Series Universal Testing Systems Brochure
Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.
- Produkte
- 06/27/2022
- 2.69 MB
ElectroPuls® E1000 All-Electric Dynamic Test Instrument
The ElectroPuls® E1000 is a state-of-the-art, all-electric test instrument designed for dynamicand static testing on a wide range of materials and components. It includes Instron® advanceddigital control electronics, DynacellTM load cell, Console software, and the very latest in testingtechnology – hassle-free tuning based on specimen stiffness, electrically operated crossheadlifts, a T-slot table for flexible test set ups, and a host of other user-orientated features. Poweredfrom a single-phase supply it requires no additional utilities for basic machine operation (forexample, pneumatic air, hydraulics, or water).
- Produkte
- 02/06/2025
- 378.09 KB
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.
- Produkte
- 02/26/2017
- 3.76 MB