EN 1939 Peel Adhesion Self Adhesive Tapes
EN 1939 is used to measure the peel adhesion properties of self-adhesive tapes. The adhesive materials are cut into 24 mm wide specimens and peeled away from the substrate at a 180° angle. EN 1939 is divided into four sections, which describe the adhesion to stainless steel, to backing material, to a liner, and for double-sided tape. The standard also describes methods to perform the peel at low temperatures and at a 90° angle. The test results in a peel strength, generally presented in an average load divided by the specimen width.
The challenges of testing to this standard are:
- Compliance with the standard
- Data rate used to capture peaks and troughs
- Gripping materials of varying thickness
- Eliminating slippage throughout the test
Instron Solution:
- Compliance with the standard – Bluehill® Universal comes with pre-configured test methods and supporting documentation to ensure that you are testing according to EN 1939.
- Data rate used to capture peaks and troughs – Instron’s 5900 series frames enable data capture of up to 2.5 kHz to ensure that all fast changing test events are captured. Too low of a bandwidth may “dull” the system and lead to missed peaks and troughs, resulting in lower average strength values.
- Gripping materials of varying thickness – When testing an adhesive to a thick substrate, standard grips can result in a misaligned specimen. The advanced screw action grips can be adjusted and offset to ensure that the specimen remains centered in the load string.
- Eliminating slippage throughout the test – The advanced screw action grips employ a patented “quick-change” jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials. Pneumatic grips can also be used for thinner substrates and are able to maintain consistent gripping pressure throughout the test.
2710 Series Screw Side Action Grips
Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.
- Produkte
- 06/28/2017
- 1.29 MB
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.
- Produkte
- 02/26/2017
- 3.76 MB
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Produkte
- 02/10/2020
- 8.35 MB
3400 Series Universal Testing Systems Brochure
Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.
- Produkte
- 06/27/2022
- 4.88 MB