Productos » Accesorios de ensayo » Mordazas de tracción » Compact Tension Fixtures for Fracture Mechanics » Compact Tension Fixtures for 12.5mm Thick Compact Tension Specimens

Compact Tension Fixtures for 12.5mm Thick Compact Tension Specimens

2780-118 | Compact Tension Fixtures for 12.5mm Thick Compact Tension Specimens

Designed in accordance with international standards such as ASTM E399, E647 & E1820

Rated Capacity: ±10kN Dynamic, 20kN Static

Temperature Range: -50 to 315°C

Includes:

  • Piston rod extender to reduce the minimum daylight between Loadcell and ±75mm actuator at mid-stroke to allow compact tension fixtures to touch (Quantity 1).
  • Fatigue Rated Adaptors. M30 x2 right hand male to male stud with preloading wedge washers (Quantity 2)

Note: Requires 2780-120 for use with a standard 3119-600 Series Chamber

Tabla de especificaciones
Capacity ±10 dynamic, 20 static kN ( ±2200 dynamic, 4500 static lbf)
Specimen Width 12.5 mm (0.49 in)
Testing Standards ASTM E399, ASTM E647, ASTM E1820 ( )