ISO » ISO 1421:1998 Determination of Tensile Strength and Elongation at Break

ISO 1421:1998 Determination of Tensile Strength and Elongation at Break

This ISO method is used to test a range of fabrics, including woven fabrics, coated fabrics, rubber-coated fabrics, and plastic-coated fabrics. There are two sub-methods used in ISO 1421, differentiated by the specimen type being used and the desired results.

Method 1, called the Strip Test, uses strip-type specimens, and is used to determine the tensile strength and elongation at break. In the strip method, the full width of the test piece is gripped in the jaws.

Method 2, called the Grab Test, is a method for the determination of tensile strength only, and only the central part of the width of the test piece is gripped in the jaws.

For both tests, it is important to have a test data sampling rate to the PC for analysis as high as 100 Hz to ensure the capture a high number of data points.

The challenges of testing to this standard are:

  • Data capture
  • Specimen gripping

 

Instron's Solution:

  • Rapid data capture rate with Instron's 5900 controller allows data peaks and valleys to be captured accurately at up to 2,500 points per second
  • Instron pneumatic side action grips with wave profile faces are well-suited to gripping stronger fabric specimens for this test while maintaining high throughput

 

It is important to review ISO 1421:1998 in order to fully understand the test setup, procedure, and results requirements.

Literature

2712-04x Series Pneumatic Side Action Grips Data Sheet

Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.

  • Productos
  • 03/22/2022
  • 1.13 MB

2710 Series Screw Side Action Grips

Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.

  • Productos
  • 06/28/2017
  • 1.29 MB

  • 01/01/1970

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Productos
  • 02/26/2017
  • 3.76 MB