ISO » ISO 813 Adhesion Strength of Rubber to Rigid Substrates

ISO 813 Adhesion Strength of Rubber to Rigid Substrates

The ISO 813 method is used to determine adhesive strength between a vulcanized or thermoplastic rubber to a rigid substrate. The test is performed at a peel angle of 90° with a speed of 50 mm/min. The adhered rubber is pulled from the rigid substrate to measure the adhesive strength, also known as the average force divided by the specimen width.

The challenges of testing to this standard are:

  • Maintaining 90° angle throughout the test
  • Bandwidth and data rate to capture peaks and troughs
  • Eliminating slippage throughout the test

 

 Instron Solution:

  • Maintaining a 90° angle throughout the test – The 90° peel fixture is able to maintain this angle by using a low force sliding table that is adjusted throughout the test. The fixture consists of a bearing mounted table, which is linked to the test system via a cable and pulley, as well as anchored on the back by a dampening coil spring. As the crosshead is driven in the tensile direction, the cable pulls the table to maintain a constant 90° angle peel, and the coil spring keeps the table from reacting to inertia caused by load peaks and troughs. This fixture is adaptable for both single and dual column frames. 
  • Bandwidth and data rate to capture peaks and troughs – Instron 6800 Series frames have multiple data bandwidth options which provide flexibility especially when acquiring fast changing data on events that occur rapidly. Instron 5900 Series frames also enable data capture of up to 2.5kHz to ensure that all fast changing events are captured. If bandwidth and data capture rate are too low, this can lead to missed peaks and troughs, resulting in lower average strength values.
  • Eliminating slippage throughout the test – Pneumatic side action grips are recommended for peel testing as they are able to maintain constant gripping pressure throughout the test. The grips employ a patented quick-change jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials.

 

Literature

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Productos
  • 02/26/2017
  • 3.76 MB

90° Angle Peel Fixture (2820-035)

Both the 90° peel test fixture and the variable angle peel test fixture consist of a bearing-mounted sled that is linked to the testing machine’s crosshead by a cable and pulley system.

  • Productos
  • 10/10/2018
  • 590.73 KB

2712-04x Series Pneumatic Side Action Grips Data Sheet

Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.

  • Productos
  • 03/22/2022
  • 1.13 MB

2710 Series Screw Side Action Grips

Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.

  • Productos
  • 06/28/2017
  • 1.29 MB