This custom-made prismatic battery weld test fixture features a cantilever style hook and alignment fixture for testing the cumulative welding of anode/cathode tabs to their respective current collector. It is also paired with a crosshead extension to provide more space behind and around the specimen/alignment device when using a single column frame. By using the alignment fixture, an operator can ensure the prismatic cell is properly gripped in an upper grip. Fixturing can also be easily swapped out to accommodate different sized prismatic cells and/or welds.