Wood Shear Testing
The determination of shear strength properties of various species of wood and adhesive bonds in wood by compressive loading are commonly established by performing large number of tests on small specimens, which are representatives of their parental materials.
Adhesives are commonly used in the wood industry for bonding thin layers of wood together to form plywood or as a quick and efficient method of joining various parts together. Since wood failure frequently occurs in bonded joints, it is therefore desirable to evaluate the shear performance of these adhesive bonds when they are subjected to compressive loads. Some of the common international standards governing shear testing of wood and adhesive bonds in wood include ASTM D143, ASTM D905, ISO 6238, JIS K6802, JIS Z2117, BS 373, and JAS 601.
A suitable test set up for these tests includes a 3300 Series electromechanical testing machine, configured with a 50 kN load cell and the wood shear fixture. As in ASTM D143, the shear fixture should apply load to the test specimen through adjustable seat to ensure uniform lateral distribution of load. In addition, the JIS standards specify that specimen should be held in position firmly during the test.
It is challenging to design fixtures that are capable of meeting the different technical aspects set by various standards. For example, ASTM D143 states that the shear tool must provide a 3 mm offset between the inner edge of the supporting surface and the plane of the adjacent edge of the loading surface, while JIS K6802 requires this shear line to be offset by 2 mm.
To meet the different offset requirements set by multiple standards, the fixture should be supplied with clearance adjustment shims to allow the clearance along the shear line to be adjusted according to the
We recommend using our Bluehill® materials testing software for setting up the test. It allows you easy configuration of different testing parameters in order to meet the specific test standards, and the software provides the result calculations required by most testing standards.
We recommend that you review the standards to fully understand its requirements.
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.
- 产品
- 02/26/2017
- 3.76 MB
3400 Series Universal Testing Systems Brochure
Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.
- 产品
- 06/27/2022
- 2.69 MB
Shear Test Fixture For Wood | 2820-060
The 2820-060 wood shear fixture is designed for testing shear strength properties of wood or adhesive bonds in wood by compression loading. The fixture consists of a high-strength steel body with a sliding, self-aligning anvil which is used to apply compressive loading to the specimen in shear. The shear line can be set at 0.0 mm, 2.0 mm or 3.0 mm by using shims. The shims are clearly engraved with the applicable standard and are easy and quick to change. The fixture is attached to the test system using simple clevis pin interfaces which allow quick and easy fitting and removal.
- 产品
- 12/23/2005
- 495.85 KB