Composite Tensile Grip Guide

Productos » Accesorios de ensayo » Composite Test Fixtures » Composite Tensile Grip Guide

This composite tensile grip guide provides an overview of key specifications for tensile grips that are ideally suited for testing composite materials. For a detailed look at the requirements and important issues related to gripping composite laminate coupons, read our Composites Gripping Guide White Paper.

Manual Wedge Action Grips
Grip Type Moving body wedge
Static Capacity 100 kN, 150 kN
Operation Manual
Interchangeable Yes
Temperature Range -70° to 315° C
Can You Attach Fixtures
Without Removing Grips? 
Some grips can be outfitted with adaptors to attach other fixtures - offering the flexibility to perform other tests without needing to remove the grips. This is referred to as piggybacking.
No
Nadcap Alignment No
Catalog Numbers 2716-002, 2716-003, 2716-008, 2736-004, 2736-005
Precision Manual Wedge Grips
Grip Type Moving body wedge
Static Capacity 100 kN, 250 kN
Operation Manual
Interchangeable Possible (not easy)
Temperature Range -80° to 250° C
Can You Attach Fixtures
Without Removing Grips? Precision Manual Wedge Grips with Composite Testing Fixture Attached
 
Some grips can be outfitted with adaptors to attach other fixtures - offering the flexibility to perform other tests without needing to remove the grips. This is referred to as piggybacking.
Yes
Nadcap Alignment Yes
Catalog Numbers 2716-028, 2716-030

Hydraulic Wedge Action Grips
Grip Type Moving body wedge
Static Capacity 130 kN, 312 kN, 600 kN
Operation Hydraulic
Interchangeable No
Temperature Range Ambient only
Can You Attach Fixtures
Without Removing Grips? Hydraulic Wedge Action Grips with Compression Fixture Attached
 
Some grips can be outfitted with adaptors to attach other fixtures - offering the flexibility to perform other tests without needing to remove the grips. This is referred to as piggybacking.
Yes
Nadcap Alignment Yes
Catalog Numbers 2743-401, 2742-501, 2742-601
Extended Hydraulic Wedge Action Grips

Extended Hydraulic Wedge Grips
Grip Type Extended moving body wedge
Static Capacity 130 kN, 312 kN
Operation Hydraulic
Interchangeable No
Temperature Range -70° to 350° C
Can You Attach Fixtures
Without Removing Grips? Extended Hydraulic Wedge Grips with Test Fixture Attached
 
Some grips can be outfitted with adaptors to attach other fixtures - offering the flexibility to perform other tests without needing to remove the grips. This is referred to as piggybacking.
Yes
Nadcap Alignment Yes
Catalog Numbers CP104947, CP109120