marzo 18, 2015

Supporting Science, Technology, Engineering, and Mathematics (STEM) Programs

Supporting Science, Technology, Engineering, and Mathematics (STEM) Programs

Supporting Science, Technology, Engineering, and Mathematics (STEM) Programs Recently, the Instron team had the honor of visiting local schools to support their Science, Technology, Engineering, and Mathematics (STEM) programs. At […]

febrero 23, 2015

The MPX Series of Motorized Pendulum Impact Testers: An Interview with Matthew Spiret

The MPX Series of Motorized Pendulum Impact Testers: An Interview with Matthew Spiret

The MPX Series of Motorized Pendulum Impact Testers: An Interview with Matthew Spiret By Stuart Milne Matthew Spiret, Sales and Product Support Engineer, talks to AZoM.com about the new MPX […]

enero 21, 2015

Is This the Next Generation of Smartphone Cases?

Is This the Next Generation of Smartphone Cases?

Is This the Next Generation of Smartphone Cases? In ASM International’s recent article, the publication discusses an exciting development happening at Yale University. The team researching mechanical engineering and materials […]

noviembre 24, 2014

Consejos y trucos para el ensayo de envases y embalajes

Consejos y trucos para el ensayo de envases y embalajes

Explore las mejores prácticas para proporcionar mejor información cuantitativa sobre la resistencia al desgarro, la resistencia a la perforación, la resistencia al pelado, la resistencia de la soldadura térmica y la durabilidad de los materiales utilizados en envases y embalajes flexibles y rígidos, y productos de envasado terminados.

noviembre 21, 2014

Helping to Standardize High-Rate Testing of Composites

Helping to Standardize High-Rate Testing of Composites

Helping to Standardize High-Rate Testing of Composites Instron has joined a new international group that is seeking to develop a best practice guide and test standards specifically for testing composites […]

noviembre 5, 2014

Question From a Customer: Air Bubbles in Extrudate

Question From a Customer: Air Bubbles in Extrudate

Question From a Customer: Air Bubbles in Extrudate Elena Mangano Q: We have an MF30 Melt Flow Indexer and started running tests on various polymers in our lab. Some of […]

noviembre 5, 2014

Challenges of Rigorous Demands

Challenges of Rigorous Demands

Challenges of Rigorous Demands Leonardo Martinez The world of materials testing is changing materials are getting stronger, stiffer, and lighter test standards are becoming stricter testing labs are asked to […]

octubre 15, 2014

Evaluating the Quality of High Performance Plastics Molding

Evaluating the Quality of High Performance Plastics Molding

Evaluating the Quality of High Performance Plastics Molding When chemical companies invest in developing high-performance polymers-such as filled polyesters, PA, PC, LCP, and PEEK-to engineer automotive and electronic components, they […]

octubre 8, 2014

Is Design Validation Slowing Down Your Time To Market?

Is Design Validation Slowing Down Your Time To Market?

Is Design Validation Slowing Down Your Time To Market? Elayne (Schneebacher) Gordonov Instron interacts with many new product development labs that have a need to validate their new product or […]