ASTM D695 / ISO 604: Compressive Properties of Rigid Plastics

ASTM D695 obtains the properties of a material's compressive strength, compressive yield point, and modulus. The standard specimen for strength determination is a right cylinder or prism whose length is twice its principal width or diameter. If the specimen is too thin, an anti-buckling support jig should be used to prevent the specimen from buckling.

ISO 604 is an international standardized test method used to determine the compressive properties of rigid and semi-rigid thermoplastic or thermoset materials. Using compression platens to apply a force, the properties obtained are compressive strength, strain at compressive strength, compressive yield stress, and if required, modulus. ISO 604 is used alongside its tensile test standard equivalent, ISO 527, and together they provide the fundamental material properties of polymers that are found in every industry and every household around the globe.

Depending on the maximum expected forces, ASTM D695 and ISO 604 can be performed on either a single column or dual column universal testing machine such as those available in Instron's 3400 and 6800 Series.

Vídeos relacionados