Prodotti » Accessori ai sistemi di prova » Estensimetri per l’apertura di cricca (COD) » Crack Opening Displacement (COD) Gauge 5/2

Crack Opening Displacement (COD) Gauge 5/2

2670-130 | Crack Opening Displacement (COD) Gauge 5/2

  • Gauge Length: 5mm (0.197inches)
  • Travel: 2mm (0.079inches)
  • Temperature range: -200°C to +200°C (-328°F to +392°F)
  • Complies to the requirements of ASTM E399-09
Letteratura

2670 Series COD Gauges

Instron® Crack Opening Displacement transducers are designed
specifically to perform standard ASTM and ISO fracture mechanics
tests (both cyclic and static), covering all common specimen
geometries (CT, SEB, Centre Crack, Arc Shaped).
Each model offers class leading linearity, whilst being rugged
enough to withstand the high energy release common in many
of these applications and can be used at both elevated and sub
ambient temperatures.
These gauges comply with requirements laid down in ASTM E399-09.