ISO 10319 Non-Contact Extensometry for Geosynthetics

Geosynthetic materials are used in a wide variety of applications within civil engineering, most often to provide strength to unstable surfaces. One use of geosynthetics is debris capture, for example on construction sites where explosives are being used or in cities where construction debris must be contained. 

Geotextiles and geosynthetics are essentially composite sheets made up of a mixture of traditional textiles as well as both oil- and bio-based plastics.

ISO 10319 is a test method for determining the tensile properties of geosynthetic materials using 200 mm wide strips. The strength of these materials combined with the geometry of the specimen can prove difficult to grip with traditional methods. Instron’s solution is capstan-style grips that prevent jaw breaks and slippage.

Traditional contacting extensometry has always been difficult with textiles of any sort, and geotextiles are no different. In fact, due to the difficulties of contacting extensometers, many companies testing these materials simply rely on crosshead displacement for strain measurement. This method is less accurate than a dedicated strain measurement device.

Instron has a non-contacting solution that addresses this problem. The AVE 2 and SVE 2 optical extensometers measure elongation by tracking marks on the specimen. This method avoids any mechanical influence on strain data which can be an issue when using contacting extensometry.

The challenges of testing to this standard are:

  • Extensometry
  • Specimen gripping

Solution:

  • Instron’s non-contacting AVE 2 optical extensometer is well-suited for measuring strain on geosynthetic specimens without mechanically influencing the results
  • Capstan grips allow for proper specimen gripping while eliminating slippage and jaw breaks, and are available in capacities up to 50 kN

It is important to review ISO 10319:2015 in order to fully understand the test setup, procedure, and results requirements. 

Literature

Webbing Capstan Grips | 2715-003

Webbing capstan grips are designed to permit faster, easier testing of seat belts and other high-strength belts and tapes. These grips are designed to permit predetermination of specimen length and allow quick, convenient loading.

  • āļœāļĨāļīāļ•āļ āļąāļ“āļ‘āđŒ
  • 12/21/2021
  • 354.41 KB

AVE 2 Non-Contacting Video Extensometer

The second generation Advanced Video Extensometer (AVE 2) utilizes patented measurement technology in the fastest, most accurate non-contacting strain measurement device commercially available.

  • āļœāļĨāļīāļ•āļ āļąāļ“āļ‘āđŒ
  • 01/26/2018
  • 1.4 MB

SVE 2 | Non-Contacting Video Extensometer Data Sheet

While contacting extensometers offer accurate strain measurement, they can have an adverse effect on results due to influence or slippage on the specimen by knife edges, damage to the specimen at break, or wear of moving parts. As a result, InstronÂŪ introduced the first commercial video extensometer in 1991. The newest Standard Video Extensometer (SVE 2) is a high-performance, non-contacting extensometer that is ideally suited for everyday applications such as rubber, soft plastics, elastomers and other materials with high strain to failure. Additionally, the SVE 2 is available with various Fields of View (FOV) that suit applications in both ambient and non-ambient temperature conditions.

  • āļœāļĨāļīāļ•āļ āļąāļ“āļ‘āđŒ
  • 12/11/2014
  • 414.47 KB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • āļœāļĨāļīāļ•āļ āļąāļ“āļ‘āđŒ
  • 02/10/2020
  • 4.15 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • āļœāļĨāļīāļ•āļ āļąāļ“āļ‘āđŒ
  • 06/27/2022
  • 2.69 MB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • āļœāļĨāļīāļ•āļ āļąāļ“āļ‘āđŒ
  • 02/26/2017
  • 3.76 MB