ISO 16402 Flexural Testing of Acrylic Resin Cements Used in Orthopaedics
During the implantation process, bone cements are used to fill the space between the implant and the bone, and their long-term mechanical stability is essential for success of the implant. By undertaking static and cyclic loading, the mechanical performance of these bone cements can be established.
ISO 16402 ‘Implants for surgery – Acrylic resin cement - Flexural fatigue testing of acrylic resin cements used in orthopaedics’ provides a guideline for flexural testing of these cements in a laboratory situation. It consists of a method for both quasi-static bend testing and flexural fatigue.
A miniature 4-point bend fixture is used within into a fluid bath filled with Ringer’s solution and maintained at 37° C. After a quasi-static bend test is performed, fatigue testing is carried out to generate a Stress level/Number of cycles (S/N) curve.
We recommend the use of either an ElectroPuls™ All-Electric Dynamic Test Instrument or 8870 servohydraulic fatigue test system for undertaking both the quasi-static and the cyclic loading of these bone cements.
We recommend that you review the standard to fully understand its requirements.
Instron has a variety of solutions for testing of orthopedic implants and devices or biomaterials.
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Prodotti
- 02/10/2020
- 4.15 MB
Orthopaedics & Devices for Osteosynthesis
Instron® has considerable experience of mechanical testing in orthopaedics: from basic static testing of raw materials, to impact loading of joint components, through to complete simulation for evaluating the fatigue and wear properties in vivo. Through every phase of implant development, our solutions meet a vast array of demands found within the orthopaedics field. These include hip and knee implants, spinal devices, and medical devices for trauma and osteosynthesis.
- Applications
- 01/16/2019
- 821.27 KB
ElectroPuls® E1000 All-Electric Dynamic Test Instrument
The ElectroPuls® E1000 is a state-of-the-art, all-electric test instrument designed for dynamicand static testing on a wide range of materials and components. It includes Instron® advanceddigital control electronics, DynacellTM load cell, Console software, and the very latest in testingtechnology – hassle-free tuning based on specimen stiffness, electrically operated crossheadlifts, a T-slot table for flexible test set ups, and a host of other user-orientated features. Poweredfrom a single-phase supply it requires no additional utilities for basic machine operation (forexample, pneumatic air, hydraulics, or water).
- Prodotti
- 02/06/2025
- 378.09 KB